Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model
JoVE 신문
공학
This content is Free Access.
JoVE 신문 공학
Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model

Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model

11,575 Views

11:10 min

May 23, 2018

DOI:

11:10 min
May 23, 2018

3 Views
, ,

Summary

Automatically generated

Thin films (100-1000 Å) of vanadium dioxide (VO2) were created by atomic-layer deposition (ALD) on sapphire substrates. Following this, the optical properties were characterized through the metal-insulator transition of VO2. From the measured optical properties, a model was created to describe the tunable refractive index of VO2.