Nanoporous gold with a hierarchical and bimodal pore size distribution can be produced by combining electrochemical and chemical dealloying. The composition of the alloy can be monitored via EDS-SEM examination as the dealloying process advances. The material's loading capacity can be determined by studying protein adsorption onto the material.