Here, we present a protocol to synthesize two metal chalcogenides (Cu1.8S and SnSe) suitable for thermoelectrics via an ultrafast (second-range), solvent-free, and one-step mechanochemical synthesis using elemental precursors. Simultaneously, we demonstrate the monitoring of the temperature in the jar during planetary ball milling in situ by the newly developed device.